Weldability Improver Ferro Vanadium

Weldability Improver Ferro Vanadium

When Weldability Improver ferrovanadium is added to steel, it promotes the formation of fine-grained structures and refines the microstructure around the weld zone. This helps to reduce the likelih...

Whatsapp Send Email
DESCRIPTION

When Weldability Improver ferrovanadium is added to steel, it promotes the formation of fine-grained structures and refines the microstructure around the weld zone. This helps to reduce the likelihood of defects, such as cracks and porosity, during welding. The presence of vanadium in the alloy enhances the steel’s ability to withstand the thermal stresses and strain associated with the welding process.

Moreover, vanadium in Weldability Improver ferrovanadium improves the mechanical properties of the welded joints, including their strength and toughness. It also aids in preventing the formation of brittle phases that can lead to weld failures. By enhancing the weldability of steels, this alloy ensures stronger and more reliable welded connections, contributing to the overall integrity of structures and components.

 FeV composition (%)
Grade V Al P Si C
FeV40-A 38-45 1.5 0.09 2.00 0.60
FeV40-B 38-45 2.0 0.15 3.00 0.80